For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ240160
Run/Test Number: L4249A
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideGA6-A
Glaze Outside – GA6-C
Clay BodyL4249A MNS
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 127 mm (5.0 in)
Height – 124 mm (4.9 in)
Weight – 425 grams (15.0 oz)

Registration Page: https://digitalfire.com/potterytony/2373