Folded silky black M340GS stoneware mug

$40.00

Folded silky black M340GS stoneware mug

SKU: AJ24009 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24009
Run/Test Number: P6819
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideGA6-B
Glaze OutsideG2934Y Black
Clay Body – M340GS
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 98 mm (3.9 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 100 mm (3.9 in)
Weight – 309 grams (10.9 oz)

Registration Page: https://digitalfire.com/potterytony/2366

Weight 309 g
Dimensions 130.00 × 98.00 × 100.00 mm