For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24011
Run/Test Number: P6851
Technique: Hand-rolled, embossed and assembled, liner-glazed inside, dip-glazed outside
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – GA6-B
Glaze Outside – GA6-C
Clay Body – M332
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 99 mm (3.9 in)
Depth at rim (including handle) – 135 mm (5.3 in)
Height – 102 mm (4.0 in)
Weight – 350 grams (12.3 oz)
Registration Page: https://digitalfire.com/potterytony/2369