Dark honey-glazed MNS mug

$45.00

Dark honey-glazed MNS mug

SKU: AJ240150 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ240150
Run/Test Number: L4208C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2826B
Glaze OutsideGA6-B
Clay BodyL4208C MNS
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 125 mm (4.9 in)
Height – 103 mm (4.1 in)
Weight – 378 grams (13.3 oz)

Registration Page: https://digitalfire.com/potterytony/2371

Weight 378 g
Dimensions 125.00 × 96.00 × 103.00 mm