Bamboo Silky Matte H550 mug

$35.00

Bamboo Silky Matte H550 mug

SKU: AJ24030 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24030
Run/Test Number: P6816
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG1947U
Glaze OutsideG2571B
EngobeL3954N
Clay BodyH550
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 111 mm (4.4 in)
Depth at rim (including handle) – 129 mm (5.1 in)
Height – 113 mm (4.4 in)
Weight – 404 grams (14.2 oz)

Registration Page: https://digitalfire.com/potterytony/2385

Weight 404 g
Dimensions 129.00 × 111.00 × 113.00 mm