Gun metal black MNP porcelain mug

$45.00

Gun metal black MNP porcelain mug

SKU: AJ24352 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24352
Run/Test Number: L4486A
Technique: Thrown, incised, pour-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing ScheduleC5DHSC
TemperatureCone 5
Glaze InsideL3500G
Glaze OutsideG2934Y gunmetal
Clay Body – L4486A MNP
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 94 mm (3.7 in)
Depth at rim (including handle) – 132 mm (5.2 in)
Height – 111 mm (4.4 in)
Weight – 354 grams (12.5 oz)

Registration Page: https://digitalfire.com/potterytony/2494

Weight 354 g
Dimensions 132.00 × 94.00 × 111.00 mm