For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24344
Run/Test Number: L4239
Technique: Jiggered, liner-glazed inside, dip-glazed outside, cast handle

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG1947U
Glaze OutsideG2571A bamboo matte
Clay BodyH550 Casting
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 94 mm (3.7 in)
Depth at rim (including handle) – 123 mm (4.8 in)
Height – 110 mm (4.3 in)
Weight – 397 grams (14.0 oz)

Registration Page: https://digitalfire.com/potterytony/2487

Weight 397 g
Dimensions 123.00 × 94.00 × 110.00 mm