Black and white incised stoneware mug

$40.00

Black and white incised stoneware mug

SKU: AJ24053 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24053
Run/Test Number: P6732
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideGR10-C
EngobeL3954N
Clay BodyH550
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 101 mm (4.0 in)
Depth at rim (including handle) – 136 mm (5.4 in)
Height – 121 mm (4.8 in)
Weight – 388 grams (13.7 oz)

Registration Page: https://digitalfire.com/potterytony/2342

Weight 388 g