Orange Polar Ice porcelain mug

$45.00

Orange Polar Ice porcelain mug

SKU: AJ24042 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24042
Run/Test Number: P6746
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG2934Y Orange
Clay BodyPolar Ice
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 91 mm (3.6 in)
Depth at rim (including handle) – 121 mm (4.8 in)
Height – 123 mm (4.8 in)
Weight – 364 grams (12.8 oz)

Registration Page: https://digitalfire.com/potterytony/2348

Weight 364 g
Dimensions 121.00 × 91.00 × 123.00 mm