For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24051
Run/Test Number: L4115J1
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – G2926B
Glaze Outside – GA6-B
Clay Body – 3D
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 105 mm (4.1 in)
Weight – 347 grams (12.2 oz)
Registration Page: https://digitalfire.com/potterytony/2350