Rutile blue buff stoneware mug

$35.00

Rutile blue buff stoneware mug

SKU: AJ24054 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24054
Run/Test Number: P6770
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideGA6-C
Glaze Outside – GA6-C
EngobeL3954B
Clay BodyM340
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 119 mm (4.7 in)
Weight – 478 grams (16.8 oz)

Registration Page: https://digitalfire.com/potterytony/2354

Weight 478 g
Dimensions 130.00 × 100.00 × 119.00 mm