Pink Crystal Matte H550 Small Mug

$30.00

Pink Crystal Matte H550 Small Mug

SKU: AJ24134 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24134
Run/Test Number: P6816
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG2571A
Glaze OutsideG2571D
Clay BodyH550
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 88 mm (3.5 in)
Depth at rim (including handle) – 117 mm (4.6 in)
Height – 96 mm (3.8 in)
Weight – 334 grams (11.8 oz)

Registration Page: https://digitalfire.com/potterytony/2393

Weight 334 g
Dimensions 117.00 × 88.00 × 96.00 mm