Pink Crystal Matte H555 mug

$35.00

Pink Crystal Matte H555 mug

SKU: AJ24035 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24035
Run/Test Number: P6842
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG1947U
Glaze OutsideG2571D
Clay BodyH555
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 116 mm (4.6 in)
Depth at rim (including handle) – 131 mm (5.2 in)
Height – 114 mm (4.5 in)
Weight – 375 grams (13.2 oz)

Registration Page: https://digitalfire.com/potterytony/2386

Weight 375 g
Dimensions 131.00 × 116.00 × 114.00 mm