Copper blue-green Polar Ice translucent porcelain mug

$30.00

Copper blue-green Polar Ice translucent porcelain mug

SKU: AJ24160 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24160
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG3806C
Clay BodyPolar Ice
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 80 mm (3.1 in)
Depth at rim (including handle) – 114 mm (4.5 in)
Height – 108 mm (4.3 in)
Weight – 284 grams (10.0 oz)

Registration Page: https://digitalfire.com/potterytony/2404

Weight 284 g
Dimensions 114.00 × 80.00 × 108.00 mm