Rutile blue brown stoneware mug

$35.00

Rutile blue brown stoneware mug

SKU: AJ24078 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24078
Run/Test Number: P6823
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze Inside – L3500G+2Fe
Glaze OutsideGA6-C
Clay BodyM350
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 88 mm (3.5 in)
Depth at rim (including handle) – 117 mm (4.6 in)
Height – 109 mm (4.3 in)
Weight – 392 grams (13.8 oz)

Registration Page: https://digitalfire.com/potterytony/2416

Weight 392 g
Dimensions 117.00 × 88.00 × 109.00 mm