For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24171
Run/Test Number: L4115J1
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideGA6-B
Clay Body – 3D+Ball Clay, bentonite, Nepheline
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 98 mm (3.9 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 97 mm (3.8 in)
Weight – 324 grams (11.4 oz)

Registration Page: https://digitalfire.com/potterytony/2406