Run/Test Number: L4283
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideGA6-B
Clay Body – L4283 MNP
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 87 mm (3.4 in)
Depth at rim (including handle) – 120 mm (4.7 in)
Height – 90 mm (3.5 in)
Weight – 271 grams (9.6 oz)