Porcelain reduction-fired mug

$35.00

Porcelain reduction-fired mug

SKU: AJ24083 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24083
Run/Test Number: P6572
Technique: Thrown, incised, dip-glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG1947U
Glaze OutsideG1947U
Clay BodyP700
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 89 mm (3.5 in)
Depth at rim (including handle) – 120 mm (4.7 in)
Height – 109 mm (4.3 in)
Weight – 302 grams (10.6 oz)

Registration Page: https://digitalfire.com/potterytony/2433

Weight 302 g
Dimensions 120.00 × 89.00 × 109.00 mm