Black stoneware mug

$35.00

Black stoneware mug

SKU: AJ24308 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24308
Run/Test Number: L4115J3S
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG2934Y Black
Clay Body – M340S Test
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 101 mm (4.0 in)
Depth at rim (including handle) – 134 mm (5.3 in)
Height – 110 mm (4.3 in)
Weight – 354 grams (12.5 oz)

Registration Page: https://digitalfire.com/potterytony/2454

Weight 354 g
Dimensions 134.00 × 101.00 × 110.00 mm