Black matte/glossy porcelain mug

$40.00

Black matte/glossy porcelain mug

SKU: AJ24310 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24310
Run/Test Number: P6928
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG3914A
Glaze OutsideG2934Y Black
Clay BodyM370
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 107 mm (4.2 in)
Depth at rim (including handle) – 137 mm (5.4 in)
Height – 124 mm (4.9 in)
Weight – 437 grams (15.4 oz)

Registration Page: https://digitalfire.com/potterytony/2456

Weight 437 g
Dimensions 137.00 × 107.00 × 124.00 mm