Variegated glossy blue mug

$35.00

Variegated glossy blue mug

SKU: AJ24106 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24106
Run/Test Number: P6729
Technique: Thrown, incised, dip-glazed

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideGR6-M
Glaze Outside – GR6-M
Clay BodyM390
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 132 mm (5.2 in)
Height – 121 mm (4.8 in)
Weight – 409 grams (14.4 oz)

Registration Page: https://digitalfire.com/potterytony/2448

Weight 409 g
Dimensions 132.00 × 97.00 × 121.00 mm