Serial Number: AJ24328
Run/Test Number: P6901
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideGR10-C MgO matte
EngobeL3954N
Clay BodyH550
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 134 mm (5.3 in)
Height – 115 mm (4.5 in)
Weight – 405 grams (14.3 oz)

Registration Page: https://digitalfire.com/potterytony/2472