For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24350
Run/Test Number: L3924C
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed

Firing ScheduleC04PLTP
Temperature – Cone 03
Glaze InsideG2931K
Glaze OutsideG2931K
Clay BodyL3924C
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 90 mm (3.5 in)
Depth at rim (including handle) – 121 mm (4.8 in)
Height – 135 mm (5.3 in)
Weight – 380 grams (13.4 oz)

Registration Page: https://digitalfire.com/potterytony/2499

Weight 380 g
Dimensions 121.00 × 90.00 × 135.00 mm