Bamboo tan incised stoneware mug

$40.00

Bamboo tan incised stoneware mug

SKU: AJ24327 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24327
Run/Test Number: P6902
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideG2571A Bamboo
Glaze OutsideG2571A bamboo matte
EngobeL3954N
Clay Body – H450
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 112 mm (4.4 in)
Depth at rim (including handle) – 138 mm (5.4 in)
Height – 122 mm (4.8 in)
Weight – 418 grams (14.7 oz)

Registration Page: https://digitalfire.com/potterytony/2489

Weight 418 g