Bamboo tan incised stoneware mug

$35.00

H550 compatible clay body made from Flintoft, Saskatchewan ball clay and Plainsman 3D.

SKU: AJ24356 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24356
Run/Test Number: L4376A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside
Description: H550 compatible clay body made from Flintoft, Saskatchewan ball clay and Plainsman 3D.

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideG2571B bamboo matte
EngobeL3954N
Clay BodyH550
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 126 mm (5.0 in)
Height – 96 mm (3.8 in)
Weight – 298 grams (10.5 oz)

Registration Page: https://digitalfire.com/potterytony/2491

Weight 298 g
Dimensions 126.00 × 96.00 × 96.00 mm