Zero4 fritware porcelain hash-tag mug

$45.00

Zero4 fritware porcelain hash-tag mug

SKU: AJ24374 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24374
Run/Test Number: L3924J
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed

Firing ScheduleC04PLTP
TemperatureCone 04
Glaze InsideG3879C
Glaze OutsideG3879C
Clay BodyL3924J
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 86 mm (3.4 in)
Depth at rim (including handle) – 113 mm (4.4 in)
Height – 122 mm (4.8 in)
Weight – 310 grams (10.9 oz)

Registration Page: https://digitalfire.com/potterytony/2518

Weight 310 g
Dimensions 113.00 × 86.00 × 122.00 mm