Zero4 translucent fritware porcelain hash-tag mug

$50.00

Zero4 translucent fritware porcelain hash-tag mug

SKU: AJ24385 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24385
Run/Test Number: L3924J
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed

Firing ScheduleC04PLTP
TemperatureCone 04
Glaze Inside – G3978C
Glaze OutsideG3879C
Clay BodyL3924J
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 89 mm (3.5 in)
Depth at rim (including handle) – 116 mm (4.6 in)
Height – 136 mm (5.4 in)
Weight – 350 grams (12.3 oz)

Registration Page: https://digitalfire.com/potterytony/2521

Weight 350 g
Dimensions 116.00 × 89.00 × 136.00 mm