Bamboo tan incised stoneware mug

$45.00

Bamboo tan incised stoneware mug

SKU: AJ24408 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24408
Run/Test Number: P6731
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideG2571A Bamboo
EngobeL3954N
Clay Body – H450
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 101 mm (4.0 in)
Depth at rim (including handle) – 136 mm (5.4 in)
Height – 116 mm (4.6 in)
Weight – 399 grams (14.1 oz)

Registration Page: https://digitalfire.com/potterytony/2543

Weight 399 g
Dimensions 136.00 × 101.00 × 116.00 mm