White glazed speckled stoneware mug

$40.00

White glazed speckled stoneware mug

SKU: AJ24439 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24439
Run/Test Number: L4471J2
Technique: Thrown, incised, dip-glazed

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG3926B
Glaze OutsideG3926B
Clay Body – M340S
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 131 mm (5.2 in)
Height – 122 mm (4.8 in)
Weight – 369 grams (13.0 oz)

Registration Page: https://digitalfire.com/potterytony/2572

Weight 369 g
Dimensions 131.00 × 95.00 × 122.00 mm