For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24030
Run/Test Number: P6816
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C10RPL
Temperature – Cone 10R
Glaze Inside – G1947U
Glaze Outside – G2571B
Engobe – L3954N
Clay Body – H550
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 111 mm (4.4 in)
Depth at rim (including handle) – 129 mm (5.1 in)
Height – 113 mm (4.4 in)
Weight – 404 grams (14.2 oz)
Registration Page: https://digitalfire.com/potterytony/2385