For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24400
Run/Test Number: P6699
Technique: Hand-rolled and assembled, engobed inside and top outside, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C10RPL
Temperature – Cone 10R
Glaze Inside – G1947U
Glaze Outside – G2571A Bamboo
Engobe – L3954N
Clay Body – P600
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 128 mm (5.0 in)
Height – 101 mm (4.0 in)
Weight – 322 grams (11.3 oz)
Registration Page: https://digitalfire.com/potterytony/2537