Black and white incised stoneware mug

$45.00

Black and white incised stoneware mug

SKU: AJ24414 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24414
Run/Test Number: P6731
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideGR10-C
EngobeL3954N
Clay Body – H450
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 97 mm (3.8 in)
Depth at rim (including handle) – 131 mm (5.2 in)
Height – 102 mm (4.0 in)
Weight – 360 grams (12.7 oz)

Registration Page: https://digitalfire.com/potterytony/2549

Weight 360 g
Dimensions 131.00 × 97.00 × 102.00 mm