Black matte mug

$35.00

Black matte mug

SKU: AJ24434 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24434
Run/Test Number: P7027
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG3914A
Glaze OutsideG2934Y Black
EngobeL3954B
Clay BodyM370
Foot Style – Unglazed flat black engobed
Width at rim (perpendicular to handle) – 92 mm (3.6 in)
Depth at rim (including handle) – 122 mm (4.8 in)
Height – 114 mm (4.5 in)
Weight – 330 grams (11.6 oz)

Registration Page: https://digitalfire.com/potterytony/2567

Weight 330 g
Dimensions 122.00 × 92.00 × 114.00 mm