Black MNS stoneware mug

$35.00

Black MNS stoneware mug

SKU: AJ24405 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24405
Run/Test Number: L4492
Technique: Thrown, incised, dip-glazed

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG3914A
Glaze OutsideG2934
Clay Body – L4492 MNS
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 94 mm (3.7 in)
Depth at rim (including handle) – 125 mm (4.9 in)
Height – 105 mm (4.1 in)
Weight – 310 grams (10.9 oz)

Registration Page: https://digitalfire.com/potterytony/2532

Weight 310 g
Dimensions 125.00 × 94.00 × 105.00 mm