For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AH24107
Run/Test Number: P6923
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – PLC6DS
Temperature – Cone 6
Glaze Inside – G2926B
Glaze Outside – G2934Y Black
Clay Body – Polar Ice
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 102 mm (4.0 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 106 mm (4.2 in)
Weight – 347 grams (12.2 oz)
Registration Page: https://digitalfire.com/potterytony/2443