For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24303
Run/Test Number: P6923
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – PLC6DS
Temperature – Cone 6
Glaze Inside – G2926B
Glaze Outside – G2934Y Blue
Clay Body – Polar Ice
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 87 mm (3.4 in)
Depth at rim (including handle) – 115 mm (4.5 in)
Height – 111 mm (4.4 in)
Weight – 332 grams (11.7 oz)
Registration Page: https://digitalfire.com/potterytony/2451