Copper blue-green MNS stoneware mug

$30.00

Copper blue-green MNS stoneware mug

SKU: AJ24072 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24072
Run/Test Number: L4208C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG3806C
Clay BodyL4208C MNS
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 89 mm (3.5 in)
Depth at rim (including handle) – 119 mm (4.7 in)
Height – 99 mm (3.9 in)
Weight – 272 grams (9.6 oz)

Registration Page: https://digitalfire.com/potterytony/2405