Copper blue-green Polar Ice porcelain mug

$40.00

Copper blue-green Polar Ice porcelain mug

SKU: AJ24144 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24144
Run/Test Number: P6746
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG3806C
Clay BodyPolar Ice
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 88 mm (3.5 in)
Depth at rim (including handle) – 120 mm (4.7 in)
Height – 99 mm (3.9 in)
Weight – 312 grams (11.0 oz)

Registration Page: https://digitalfire.com/potterytony/2349

Weight 312 g