Copper blue-green porcelain mug

$35.00

Copper blue-green porcelain mug

SKU: AJ24067 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24067
Run/Test Number: L4283
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG3806C
Clay Body – L4283
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 81 mm (3.2 in)
Depth at rim (including handle) – 111 mm (4.4 in)
Height – 85 mm (3.3 in)
Weight – 231 grams (8.1 oz)

Registration Page: https://digitalfire.com/potterytony/2409

Weight 231 g
Dimensions 111.00 × 81.00 × 85.00 mm