Dark Glossy Honey-Glazed 3D Cone 6 Mug

$40.00

Dark Glossy Honey-Glazed 3D Cone 6 Mug

SKU: AJ24046 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24046
Run/Test Number: L4115J1
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideGA6-B
Clay Body – 3D+Ball Clay, bentonite, Nepheline
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 133 mm (5.2 in)
Height – 106 mm (4.2 in)
Weight – 332 grams (11.7 oz)

Registration Page: https://digitalfire.com/potterytony/2389

Weight 332 g
Dimensions 133.00 × 100.00 × 106.00 mm