Dark honey glazed mug

$40.00

Dark honey glazed mug

SKU: AJ24369 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24369
Run/Test Number: P6971
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B white
Glaze OutsideGA6-B
Clay BodyP300
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 127 mm (5.0 in)
Height – 118 mm (4.6 in)
Weight – 387 grams (13.6 oz)

Registration Page: https://digitalfire.com/potterytony/2510

Weight 387 g
Dimensions 127.00 × 96.00 × 118.00 mm