For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24336
Run/Test Number: L4382A
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed
Description: This H550 compatible clay body is made from Flintoft, Saskatchewan ball clay and Plainsman 3D.
Firing Schedule – C10RPL
Temperature – Cone 10R
Glaze Inside – G2571F
Glaze Outside – G2571F blue MgO matte
Engobe – L3954N
Clay Body – H550 test
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 98 mm (3.9 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 106 mm (4.2 in)
Weight – 341 grams (12.0 oz)
Registration Page: https://digitalfire.com/potterytony/2479