Floating blue MNP black porcelain mug

$40.00

Floating blue MNP black porcelain mug

SKU: AJ24436 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24436
Run/Test Number: L4484D
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideGR6-M
Clay BodyL4484D MNP Black
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 96 mm (3.8 in)
Depth at rim (including handle) – 130 mm (5.1 in)
Height – 109 mm (4.3 in)
Weight – 322 grams (11.3 oz)

Registration Page: https://digitalfire.com/potterytony/2569

Weight 322 g
Dimensions 130.00 × 96.00 × 109.00 mm