Serial Number: AJ24425
Run/Test Number: P7024
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – PLC6DS
Temperature – Cone 6
Glaze Inside – G3914A
Glaze Outside – GR6-M
Clay Body – M340
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 91 mm (3.6 in)
Depth at rim (including handle) – 122 mm (4.8 in)
Height – 104 mm (4.1 in)
Weight – 358 grams (12.6 oz)