For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24432
Run/Test Number: P7024
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – PLC6DS
Temperature – Cone 6
Glaze Inside – G3914A
Glaze Outside – GR6-M
Clay Body – M340
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 99 mm (3.9 in)
Depth at rim (including handle) – 132 mm (5.2 in)
Height – 113 mm (4.4 in)
Weight – 404 grams (14.2 oz)
Registration Page: https://digitalfire.com/potterytony/2565