For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24334
Run/Test Number: P6881
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C10RPL
Temperature – Cone 10R
Glaze Inside – G1947U
Glaze Outside – G2571E gunmetal
Clay Body – P700
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 95 mm (3.7 in)
Depth at rim (including handle) – 128 mm (5.0 in)
Height – 128 mm (5.0 in)
Weight – 392 grams (13.8 oz)
Registration Page: https://digitalfire.com/potterytony/2478