Serial Number: AJ24368
Run/Test Number: L4491
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Description: Blend of MNP and M370
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – G2926B white
Glaze Outside – GA6-B
Clay Body – MNP M370 mix
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 94 mm (3.7 in)
Depth at rim (including handle) – 123 mm (4.8 in)
Height – 116 mm (4.6 in)
Weight – 354 grams (12.5 oz)