Serial Number: AJ24402
Run/Test Number: L3905C
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – G2926B
Glaze Outside – G3914A
Clay Body – M370
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 87 mm (3.4 in)
Depth at rim (including handle) – 124 mm (4.9 in)
Height – 113 mm (4.4 in)
Weight – 297 grams (10.5 oz)