For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24376
Run/Test Number: L4484
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – GA6-B
Glaze Outside – G2934Y Red
Clay Body – L4484 MNP
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 88 mm (3.5 in)
Depth at rim (including handle) – 119 mm (4.7 in)
Height – 0 mm (0.0 in)
Weight – 320 grams (11.3 oz)
Registration Page: https://digitalfire.com/potterytony/2516