For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.
Serial Number: AJ24366
Run/Test Number: P6967
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule – C6DHSC
Temperature – Cone 6
Glaze Inside – G2926B
Glaze Outside – G2934Y red
Clay Body – Polar Ice
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 90 mm (3.5 in)
Depth at rim (including handle) – 121 mm (4.8 in)
Height – 110 mm (4.3 in)
Weight – 357 grams (12.6 oz)
Registration Page: https://digitalfire.com/potterytony/2508